Place of Origin:
Jiang Su
Brand Name:
DELLOK YONGHUI
Certification:
CE/TEMA/ASME
Model Number:
Tube Bundle
ASME SB171 C71500 Transverse Baffle, Longitudinal Baffle & Impingement Plate for Heat Exchanger Applications
Baffles are essential components of shell and tube heat exchangers, used to support and fix the tubes in a defined position. Multiple baffle configurations are available to suit different thermal and hydraulic requirements. The most common type is the perforated plate formed as a segmented circle. In segmental baffles, the segmented sections are arranged so that their faces are disposed opposite to each other along the tube bundle at specified intervals.
Our fabrication capabilities also include No Tube in Window (NTIW) baffles, helically shaped baffles, and full support baffles. We are a professional supplier of baffle plates for pressure vessel heat exchangers, heaters, condensers, reboilers, separators, and evaporators.
| Baffle Type | Single Segmental Baffle; Double Segmental Baffle; Triple Segmental Baffle; Disk and Doughnut Baffles; Orifice Baffles; Rod Baffles |
|---|---|
| Baffle Material | ASME SB171 C46400, C63000, C70600, C71500, C71640 |
Baffle spacing is generally set between 0.3 and 0.5 times the shell diameter, with 50.8 mm (2 inch) being the minimum used.
For example, with a shell diameter of 356 mm (14 inch), the minimum baffle spacing selected should be between 106.8 mm (4.2 inch) and 178 mm (7 inch).
Both values are considered valid, as they are above the minimum recommended value of 50.8 mm (2 inch).
Double segmental baffle configuration
Every tube inserted into a baffle has a clearance between the tube outside diameter and the baffle hole diameter. This clearance allows the tubes to be inserted into the baffle with ease. TEMA standards provide optimum clearance requirement values employed in industry, taking into account the spacing needed for differential expansion and contraction between the baffle plate and the tubes.
A certain amount of leakage through the clearances is permitted to reduce stagnant regions, make turbulent conditions more uniform, and reduce shell-side pressure drop. The leakage also helps reduce deposits in stagnant areas.
If the clearances are too large, excessive fluid bypassing can occur, resulting in fluid-starved regions in the shell with low fluid velocities.
| Type of Materials | Technical Requirements |
|---|---|
| Or according to customer requirement | Custom specifications available on request |
| Duplex Stainless Steel | ASTM/ASME SA240 S32205, S31803, S332750, S32760, S31254, S31500, S32304, … |
| Austenitic Stainless Steel | ASTM/ASME SA240 SS304, SS304L, SS310S, SS310H, SS316, SS316L, SS317, SS317L; ASTM/ASME SA240 SS321, SS321H, SS347, SS347H, SS904L |
| Carbon Steel | ASTM/ASME SA283 / SA285 / SA299 Gr.A, Gr.B, Gr.C, Gr.D; ASTM/ASME SA516 Gr.55, Gr.60, Gr.65, Gr.70 |
| Alloy Steel | ASTM/ASME SA387 Gr.2, Gr.11, Gr.12, Gr.21, Gr.22, Gr.5, Gr.9, Gr.91 |
| Non-Ferrous | Titanium, Brass, Al-Brass, Copper Nickel, Nickel Alloys, Hastelloy |
| Titanium | ASTM/ASME SB265 Gr.1, Gr.2, Gr.5, Gr.7, Gr.9, Gr.12, Gr.16 |
| Copper Alloy | ASTM/ASME SB171 C44300, C46400, C63000, C70600 (Cu-Ni 90/10), C71500 (Cu-Ni 70/30); ASTM/ASME SB127 Monel 400 |
| Copper | ASTM/ASME SB152 UNS C10100, C10200, C10300, C10800, C12200 |
| Aluminum Bronze | ASTM/ASME SB169 C61300, C61400 |
| Nickel Alloys | ASTM/ASME SB168 UNS N06600, N06601, N06603, N06690, N06693, N06025, N06045, N06696, UNS N06617; ASTM/ASME SB333 UNS N10001, N10665, N10675, N10629, N10624; ASTM/ASME SB409 UNS N08120, N08890, N08800, N08810, N08811; ASTM/ASME SB424 UNS N08825, N08221, N06845; ASTM/ASME SB434 UNS N10003, N10242; ASTM/ASME SB435 UNS N06002, N06230, N12160, R30556; ASTM/ASME SB443 UNS N06625, N06219; ASTM/ASME SB463 UNS N08020; ASTM/ASME SB536 UNS N08330, N08332; ASTM/ASME SB575 UNS N10276, N06022, N06455, N06035, N06044, N06058, N06059, N06200, N10362, N06210, N06686; ASTM/ASME SB582 UNS N06007, N06975, N06985, N06030; ASTM/ASME SB625 UNS N08925, N08031, N08034, N08932, N08926, N08354, N08830, R20033; ASTM/ASME SB688 UNS N08366, N08367; ASTM/ASME SB709 UNS N08028 |
| Pure Nickel | ASTM/ASME SB162 Ni200 (UNS N02200), Ni201 (UNS N02201) |
| Clad Materials | ASTM/ASME SB898, SB263, SB264 or closer; explosion cladding, making materials of 2 in 1 or 3 in 1; Titanium-Steel, Nickel-Steel, Titanium-Copper, Stainless Steel-Carbon Steel, Alloys-Steel, etc. |